Stochastic modeling of chloride-induced pitting corrosion of reinforcement bars in concrete
Journal article

Stochastic modeling of chloride-induced pitting corrosion of reinforcement bars in concrete

L Llano, MK Chryssanthopoulos, A Hagen-Zanker and MI Rafiq
Safety, Reliability, Risk and Life-Cycle Performance of Structures and Infrastructures - Proceedings of the 11th International Conference on Structural Safety and Reliability, ICOSSAR 2013, pp.2659-2664
01/12/2013